Uso de materiales alternativos para mejorar la resistencia del mortero de pega de mamposteria estructural (fibra de fique)
dc.contributor.advisor | Carvajal Ronderos, Edgard Mauricio | |
dc.contributor.author | Guzman Beltran, Sergio Alejandro | |
dc.contributor.author | Porras Gil, Maylon Stiven | |
dc.creator.degree | Tecnólogo(a) en Construcciones Arquitectónicas | spa |
dc.date.accessioned | 2020-07-09T22:30:49Z | |
dc.date.available | 2020-07-09T22:30:49Z | |
dc.date.issued | 2020 | |
dc.description | Esta investigación es tipo aplicada, con un nivel de profundización explicativo, ya que solo se recolectarán los datos en un momento dado de la investigación Adición de fibras naturales al mortero de pega en mampostería estructural; la finalidad consiste en generar una alternativa para aumentar la resistencia de los morteros de mampostería generando mayor durabilidad en las construcciones formales y en las edificaciones no formales que utilizan materiales que no cumplen con la NSR 10 y normas técnicas colombianas NTC. Este mortero se articula y se adapta especialmente a los muros de bloque y ladrillo, con un recurso fibrico de diversas regiones rurales del país. La fibra de fique se plantea ya que su utilización es económica/técnica, igualmente la paja y esterilla de coco, buscando alcanzar mejores resultados a compresión se plantea la utilización de esta materia prima. Una vez argumentando la propuesta a utilizar las diferentes mezclas de adiciones en diferentes proporciones se ejecuta varias pruebas caseras determinando sus propiedades y reacciones se procede a comparar estos resultados con el mayor beneficio. Se elaboran cubos de 5cm x 5cm con láminas en madera RH y se realiza las diferentes mezclas de mortero dosificación 1:3 con las diferentes fibras naturales, mortero mezclado en situ y mortero estructural premezclado. Las probetas se elaboran y funden en casa el día 30 de marzo de 2020 obteniendo 15 por cada elemento con un total de 75 muestras, desencofrando 24 horas después sumergiéndolos en un recipiente con agua. 15 de las muestras se proceden al fallo mediante una prensa manual de 5” a distintas edades 1,3,7,28 días con el fin de determinar su capacidad y resistencia a través del tiempo. Una vez llegando a los 28 días de secado, el 27 de abril de 2020 se procedió el fallo de los últimos especímenes, presentando un cuadro comparativo hallando la proporción y porcentaje óptimo de adición, las particularidades que mejoraron y empeoraron en las mezclas. En esta línea, fundados en el enfoque de situar de materiales de construcción con atributos, razonables y de reducido costo, se ve la necesidad de mezclar morteros para mampostería con fibras; en los que la fibra de fique interviene para aumentar su resistencia y características. Debido que en Colombia el 60% de las construcciones usan mortero mezclado en situ con pocas especificaciones técnicas generando una mayor deterioro y fallo por cortante se utilizara esta unión de materiales obteniendo una mayor resistencia similar o mayor al mortero estructural. | spa |
dc.description.abstract | This research is an applied type, with a level of explanatory depth, since the data will only be collected at a given moment in the research "Adding natural fibers to the glue mortar in structural masonry" The purpose is to generate an alternative to increase the resistance of masonry mortars generating greater durability in formal constructions and in non-formal buildings that use materials that do not comply with NSR 10 and Colombian technical standards NTC. This mortar is articulated and specially adapted to block and brick walls, with a fiber resource from various rural regions of the country. The fiber of fique arises since its use is economic / technical, likewise the straw and coconut mat, seeking to achieve better results compared to the use of this raw material. Once arguing the proposal to use the different mixtures of additions in different proportions, several home tests are carried out determining their properties and reactions. These results are compared with the greatest benefit. Cubes of 5cm x 5cm are made with sheets of rh wood and the different mortar mixes are dosed 1: 3 with the different natural fibers, mortar mixed in situ and pre-mixed structural mortar. The test tubes are made and melted at home on March 30, 2020, obtaining 15 for each element with a total of 75 samples, stripping 24 hours later, submerging them in a container with water. 15 of the samples proceed to failure using a 5” manual press at different ages 1,3,7,28 days in order to determine their capacity and resistance over time. Once reaching the 28 days of drying, on April 27, 2020 the failure of the last specimens was proceeded, presenting a comparative table finding the proportion and optimal percentage of addition, the characteristics that improved and worsened in the mixtures. In this sense, based on the focus of having quality, sustainable and low-cost construction materials, there is a need to mix masonry mortars with fibers; in which the fiber of fique intervenes to increase its resistance and properties. Due to the fact that in Colombia 60% of the constructions use mortar mixed in situ with few technical specifications, generating greater deterioration and shear failure, this union of materials will be used, obtaining a greater or similar resistance to structural mortar. | spa |
dc.identifier.uri | http://hdl.handle.net/11396/5733 | |
dc.language.iso | spa | |
dc.publisher | Universidad La Gran Colombia | spa |
dc.publisher.branch | Bogotá | spa |
dc.publisher.department | Facultad de Arquitectura | spa |
dc.publisher.program | Tecnología en Construcciones Arquitectónicas | spa |
dc.rights | Attribution-NonCommercial-NoDerivatives 4.0 International | * |
dc.rights.uri | http://creativecommons.org/licenses/by-nc-nd/4.0/ | * |
dc.subject | Mortero | spa |
dc.subject | Fique | spa |
dc.subject | Fibras | spa |
dc.subject | Falla a cortante | spa |
dc.subject | Resistencia del mortero | spa |
dc.subject.keyword | Mortar | spa |
dc.subject.keyword | Fique | spa |
dc.subject.keyword | Fibers | spa |
dc.subject.keyword | Shear failure | spa |
dc.subject.keyword | Mortar resistance | spa |
dc.subject.lemb | Fibras vegetales - Materiales de construcción | spa |
dc.subject.lemb | Mampostería | spa |
dc.subject.lemb | agregados (materiales de construcción) | spa |
dc.title | Uso de materiales alternativos para mejorar la resistencia del mortero de pega de mamposteria estructural (fibra de fique) | spa |
Archivos
Bloque original
1 - 2 de 2
Cargando...
- Nombre:
- MATERIALES ALTERNATIVOS PARA MEJORAR LA RESISTENCIA DEL MORTERO DE PEGA DE MAMPOSTERÍA ESTRUCTURAL.pdf
- Tamaño:
- 1.66 MB
- Formato:
- Adobe Portable Document Format
- Descripción:
- Trabajo de grado
No hay miniatura disponible
- Nombre:
- CARTA AUTORIZACION FIRMADA.pdf
- Tamaño:
- 641.14 KB
- Formato:
- Adobe Portable Document Format
- Descripción:
- Anexo
Bloque de licencias
1 - 1 de 1
No hay miniatura disponible
- Nombre:
- license.txt
- Tamaño:
- 3.31 KB
- Formato:
- Item-specific license agreed upon to submission
- Descripción: